B27G120 steel silicon content is about 3% to 5%, and other major iron silicon alloy. Electricity, electronics and military industries indispensable soft magnetic alloy is also the largest output of metal functional materials, mainly used for all kinds of motors, generators and transformers cores.

Εισαγωγή προϊόντος

Εισαγωγή προϊόντος

 

B27G120 electrical steel has a high magnetic permeability, low core loss, and excellent magnetic properties, making it ideal for use in high-efficiency transformers and other electromagnetic devices. It also has a relatively low coercivity, which means it is easy to magnetize and demagnetize, making it ideal for applications that require rapid switching or modulation of magnetic fields.

GNEE B27G120 Electrical Silicon Steel CRGO Steel Sheet of Transformer

B27G120

0.23mm-0.35mm

20mm-1250mm

B27G120 Electrical steel Electromagnetic performance standard


Density (kg/dm3)

Maximum iron loss P15/50 (W/kg)

Minimum magnetic induction B50 (T)

B27G120

0.27

7.65

1.20

1.80


B27G120 oriented electrical steel Typical electromagnetic performance

Density (kg/dm3)

iron loss P15/50 (W/kg)

magnetic induction B50 (T)

P15/50

P17/50

B8

B25

B27G120

0.27

7.65

0.78

1.16

1.85

1.92

BaoSteel B27G120 Electrical steel equal grade

B27G120

27Q120

27Z120

27JG120

-

C120-27

27PG120

NV27S-120

M-4